Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Perstorp Compounds Akestra™ 90 Thermoplastic Copolyester

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Perstorp Compounds
Trade Name Akestra™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Perstorp Compounds Akestra™ 90 Thermoplastic Copolyester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Akestra™ is a thermoplastic with a sparkling glass-like appearance. It can be used as a polystyrene alternative for heat resistant thin wall containers, a polycarbonate alternative for durable “dishwasher proof” transparent products, and a glass alternative for hot-fill food containers. Akestra™ 90 is comparable to PETG in transparency, but with more than 10°C superior Tg and 20% higher flexural modulus and fully compatible with conventional PET. Information provided by Perstorp Compounds Inc.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 54.0 MPa
7830 psi
Elongation at Break 220 %
220 %
ASTM D638
Flexural Yield Strength 89.0 MPa
12900 psi
ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
ASTM D790
Izod Impact, Notched 0.250 J/cm
0.468 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 95.0 °C
203 °F
ASTM D7426
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 91 %
91 %
ASTM D1003
Users viewing this material also viewed the following: