Phillips 66 COPYLENE® CH023NX Polypropylene, Homopolymer, Thermoforming

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Phillips 66
Trade Name COPYLENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Phillips 66 COPYLENE® CH023NX Polypropylene, Homopolymer, Thermoforming.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
COPYLENE™ CH023NX has a high performance nucleation system designed to yield high clarity thermoformed articlesApplications: ThermoformingInformation provided by Phillips 66.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 2.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.9 MPa
5350 psi
(2 in/min); ASTM D638
Elongation at Yield 7.8 %
7.8 %
ASTM D638
Flexural Modulus 1.69 GPa
245 ksi
0.05 in/mm, 1% Secant, Procedure A; ASTM D790
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
Method A; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 114 °C
237 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Process Thermoforming
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution