Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Phillips Sumika Marlex® ABF-080 Thermoplastic Polyolefin  (discontinued **)

Category Polymer , Thermoplastic , Polyolefin
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Phillips Sumika Marlex® ABF-080 Thermoplastic Polyolefin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Air damInterior trimInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued prior to the shutdown announcement.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
Injection molded specimen; ASTM D1505
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
ASTM D2240
Tensile Strength, Yield 18.0 MPa
2610 psi
2 in/min, injection molded, type 1 specimen; ASTM D638
Flexural Modulus 0.550 GPa
79.8 ksi
Injection molded specimen, 0.05 in/min, Tangent method; ASTM D790
Izod Impact, Notched 1.23 J/cm

@Temperature -30.0 °C
2.30 ft-lb/in

@Temperature -22.0 °F
injection molded specimen; ASTM D256
Gardner Impact 32.8 J

@Temperature -30.0 °C
24.2 ft-lb

@Temperature -22.0 °F
ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 43.0 °C
109 °F
injection molded specimen; ASTM D648