Piezo Kinetics 906 Lead Nickel Niobate Piezoelectric

Category Ceramic , Oxide , Piezoelectric
Manufacturer Piezo Kinetics, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Piezo Kinetics 906 Lead Nickel Niobate Piezoelectric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PKI 906 is slightly different in composition than the "general" PZT formulations. Its PZT-doped Lead Nickel Niobate composition was developed to enhance the d33 and dielectric properties of Navy Type VI materials. These enhanced properties make it the optimum choice for ultrasound or actuator applications. The increased dielectric constant allows engineers to use the material in smaller (higher frequency) applications while still maintaining the desired or necessary capacitance. The increased d33 allows for higher displacement applications. Elastic Compliance s11E (x 10-12 m²/n): 15.4.Elastic Compliance s33E (x 10-12 m²/n): 18.2.Property data at 25°C. Information supplied by Piezo Kinetics, Inc.
Physical Properties Metric English Comments
Density 7.80 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 55.0 GPa
7980 ksi
Poissons Ratio 0.22
0.22
Shear Modulus 23.0 GPa
3340 ksi
calculated
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Maximum Operating Temperature
Electrical Properties Metric English Comments
Curie Temperature 150 °C
302 °F
Dielectric Constant 5500

@Frequency 1000 Hz
5500

@Frequency 1000 Hz
Dissipation Factor 0.023

@Frequency 1000 Hz
0.023

@Frequency 1000 Hz
Piezoelectric Longitudinal Coupling Factor, k33 0.70
0.70
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -310
-310
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 700
700
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 13.6
13.6
Piezoelectric Planar Coupling Factor, kp 0.60
0.60
Piezoelectric Mechanical Q 55
55
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 660
660
Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N -6.40
-6.40
Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N 14.4
14.4
Piezoelectric Transverse Coupling Factor, k31 0.35
0.35
Copyright © lookpolymers.com All Rights Reserved