Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Pinnacle Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pinnacle Polymers 2135 Impact Polypropylene Copolymer, Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties and lot-to-lot consistency.Features: Good impact strengthHigh melt flowSuperior processabilityApplications: PackagingHousewaresConsumer productsCertifications: Pinnacle's polypropylene, as marketed by Pinnacle Polymers Company, in natural, uncolored pellet form complies with appropriate requirements of CFR Title 21, Part 177, Subpart B, Section 177.1520 (c) 1.1a entitled “Olefin Polymers” of the Food Additives Amendment of 1958 to the United States Food, Drug and Cosmetic Act of 1938.Information provided by Pinnacle Polymers.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 35 g/10 min
35 g/10 min
Condition L 230/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.1 MPa

@Thickness 3.20 mm
3640 psi

@Thickness 0.126 in
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638
Elongation at Yield 11 %

@Thickness 3.20 mm
11 %

@Thickness 0.126 in
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638
Flexural Modulus 1.03 GPa

@Thickness 3.20 mm
150 ksi

@Thickness 0.126 in
At 1.27 mm/min, 1% secant, injection molded ASTM Type 1 specimen; ASTM D790A
Izod Impact, Notched 0.801 J/cm

@Thickness 3.20 mm,
Temperature 22.8 °C
1.50 ft-lb/in

@Thickness 0.126 in,
Temperature 73.0 °F
injection molded ASTM Type 1 specimen; ASTM D256