Material Notes:
Continuously processed acrylic sheet.Data provided by the manufacturer, Plaskolite, Inc.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 68
68
Method A; ASTM D785
Tensile Strength, Yield 55.0 MPa
7980 psi
ASTM D638
Tensile Modulus 2.30 GPa
334 ksi
ASTM D638
Flexural Yield Strength 83.0 MPa
12000 psi
ASTM D790
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
ASTM D256
0.200 J/cm

@Temperature -18.0 °C
0.375 ft-lb/in

@Temperature -0.400 °F
ASTM D256
Gardner Impact 3.40 J
2.51 ft-lb
J; ASTM D3029-GB, unpainted
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature -18.0 - 38.0 °C
40.0 µin/in-°F

@Temperature -0.400 - 100 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
annealed; ASTM D648
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
ASTM D1003
Transmission, Visible 92 %
92 %
ASTM D1003