Plaskolite Optix® CA-82 UVA UV-Absorbing Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, UV Stabilized, Molded
Manufacturer Plaskolite
Trade Name Optix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite Optix® CA-82 UVA UV-Absorbing Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for injection molding and contains a mold release agent. This resin offers high heat resistance and excellent stiffness/strength propertiesYellowness Index 0.6-1.4 per ASTM D1925.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Melt Flow 2.6 g/10 min
2.6 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 67.6 MPa
9800 psi
ASTM D638
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C
201 °F
ASTM D648
Vicat Softening Point 102 °C
216 °F
Rate A, ASTM D1525
Optical Properties Metric English Comments
Haze 3.0 %
3.0 %
ASTM D1003
Transmission, Visible 92 %
92 %
ASTM D1003