Plaskolite West Optix® CA-86 Clear General Purpose Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, General Purpose, Molded
Manufacturer Plaskolite West, Inc.
Trade Name Optix®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite West Optix® CA-86 Clear General Purpose Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose acrylic resin, extrusion and injection molding gradeApplications: A general-purpose acrylic resin designed for high heat application. This resin offers the highest heat resistance and stiffness among the CA acrylic resins.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Melt Flow 1.6 g/10 min
1.6 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM D638
Elongation at Break 6 %
6 %
ASTM D638
Modulus of Elasticity 3.65 GPa
529 ksi
ASTM D638
Flexural Strength 117.2 MPa
17000 psi
ASTM D790
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256
Gardner Impact 0.226 J
0.167 ft-lb
Falling Weight; ASTM D3029GB
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
UL746 ABC Relative Thermal Index
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
219 °F
ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 92 %
92 %
ASTM D1003