Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plaskolite West Optix® CA-924 Impact Modified Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Impact Modified, Molded
Manufacturer Plaskolite West, Inc.
Trade Name Optix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite West Optix® CA-924 Impact Modified Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Injection Molding Grade Pellets. Good impact strength.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Melt Flow 6.3 g/10 min
6.3 g/10 min
Condition 230/3.8; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Elongation at Break 4.6 %
4.6 %
ASTM D638
Modulus of Elasticity 3.30 GPa
479 ksi
ASTM D638
Flexural Strength 86.0 MPa
12500 psi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Gardner Impact 1.60 J
1.18 ft-lb
ASTM D3029 GB
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
181 °F
ASTM D648
Vicat Softening Point 112 °C
234 °F
ASTM D1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 91.6 %
91.6 %
Luminous Transmittance, ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 215 - 249 °C
419 - 480 °F