Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100TL NC010 is a high viscosity acetal homopolymer with 1.5% Teflon® PTFE Micropowder.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 500CL BK601 Acetal Homopolymer
(Unverified Data**) Delrin® 500CL BK601 is a medium viscosity acetal homopolymer containing a chemical lubricant, designed for low wear and friction against metals.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500AL is a medium viscosity acetal homopolymer, lubricated for low wear and /or coefficient of friction. It has been developed for consideration into applications such as parts for the fo.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG511DP is a medium viscosity acetal homopolymer, with improved thermal stability and modifications for more precise molding. It has been developed for consideration into applications such .. |
|||
Melt Temperature | 215 - 240 °C | 419 - 464 °F | |
Ineos ABS Lustran® 256 Extrusion, Blending
(discontinued **) A natural, medium-flow, medium-impact extrusion grade of ABS. It is used for blending with other Lustran ABS virgin and regrind materials to optimize cost and performance.Properties tested in trans.. |
|||
Melt Temperature | 215 - 240 °C | 419 - 464 °F | |
Ineos ABS Lustran® 456 Extrusion, Matte-Gloss
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Melt Temperature | 215 - 240 °C | 419 - 464 °F | Injection Molding |
LG Chemical KEYFLEX BT 1068D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 215 - 245 °C | 419 - 473 °F | Injection Molding |
LG Chemical KEYFLEX BT 3047D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 215 - 245 °C | 419 - 473 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 3047D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 215 - 249 °C | 419 - 480 °F | Extrusion |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
Melt Temperature | 215 °C | 419 °F | |
Polyram Polytron P40B01 Homopolymer Polypropylene, Chemically Coupled 40% LGF A chemically coupled 40% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Melt Temperature | 215 - 235 °C | 419 - 455 °F | |
Covestro Desmopan® DP 3660DU Polyurethane Extrusion- and injection molding gradetransparent up to 6 mm wall thicknesshydrolysis-stabilisedwith special UV stabilizerswith release agentgood wear resistanceApplicationSports shoe solesHosesnon-.. |
|||
Melt Temperature | 215 - 235 °C | 419 - 455 °F | |
Covestro Desmopan® DP 3690AU Polyurethane Extrusion- and injection molding gradehydrolysis-stabilisedwith special UV stabilizerswith release agenttransparent up to 6 mm wall thicknessgood wear resistanceApplicationSports shoe solesFilmsHose.. |
|||
Melt Temperature | 215 - 235 °C | 419 - 455 °F | |
Covestro Desmopan® DP 9650DU Polyurethane Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedAs of .. |
|||
Melt Temperature | 215 °C | 419 °F | 90 RPM |
Equate EMDA-6200 HDPE Blow Molding Resin EMDA-6200 grade is a high-density polyethylene copolymer resin designed for blow molding small to medium size bottles. It can be used on intermittent as well as continuous blow molding machines for .. |
|||
Melt Temperature | 215 - 225 °C | 419 - 437 °F | |
E-Polymers SEPAZ® LH40 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Melt Temperature | 215 - 250 °C | 419 - 482 °F | |
ExxonMobil Santoprene® 8291-80TB Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer which bonds to adhesive/epoxy spin-finished polyester or standard nylon fibers for closed-braid hose and woven-substrate products. With bonds strong.. |
|||
Melt Temperature | 215 - 225 °C | 419 - 437 °F | |
E-Polymers SEPAZ® LC40 PP Copolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 588P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 588P NC010 is a medium viscosity acetal homopolymer resin for injection molding. It has good thermal stability, and modifications for more precise molding (reduced warpage, good dimensiona.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 900P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing thermal stability.Information provided by DuPont Perform.. |
|||
Melt Temperature | >= 215 °C | >= 419 °F | |
Voloknohim PA 6-210/311 Nylon 6 For production of plastics and industrial goods used in machine building and motor industry. Nylon 6 bright, not dyed and (or) heat stabilizedInformation provided by Voloknokhim |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 300CP BK642 Acetal Homopolymer
(Unverified Data**) Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance. This black is formulated to mainta.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the.. |
|||
Melt Temperature | 215 - 230 °C | 419 - 446 °F | |
Eastman Tenite 525-10 CAB Cellulose Acetate Butyrate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |