Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVASTER®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
Linear Mold Shrinkage 0.0102 cm/cm
0.0102 in/in
Linear Mold Shrinkage, Transverse 0.0112 cm/cm
0.0112 in/in
Melt Flow 10 g/10 min

@Load 0.325 kg,
Temperature 270 °C
10 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
Elongation at Break 3.5 %
3.5 %
Tensile Modulus 5.00 GPa
725 ksi
Flexural Strength 115 MPa
16700 psi
Flexural Modulus 3.35 GPa
486 ksi
Charpy Impact Unnotched 3.00 J/cm²

@Temperature -20.0 °C
14.3 ft-lb/in²

@Temperature -4.00 °F
5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.500 J/cm²

@Temperature -20.0 °C
2.38 ft-lb/in²

@Temperature -4.00 °F
0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 200 - 220 °C
392 - 428 °F
Deflection Temperature at 1.8 MPa (264 psi) 170 °C
338 °F
Vicat Softening Point 205 °C
401 °F
B
Flammability, UL94 HB
HB
Glow Wire Test 750 °C
1380 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
Dielectric Strength 28.0 kV/mm
711 kV/in
Comparative Tracking Index 350 V
350 V
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F
Mold Temperature 50.0 - 80.0 °C
122 - 176 °F
Drying Temperature 120 °C
248 °F
Dry Time 4 hour
4 hour
Moisture Content 0.050 %
0.050 %
Injection Pressure 60.0 - 100 MPa
8700 - 14500 psi