PlastiComp Velocity® LGF50-PA66 High Flow Nylon 66, 50% Long Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Glass Fiber Filled
Manufacturer PlastiComp
Trade Name Velocity®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Velocity® LGF50-PA66 High Flow Nylon 66, 50% Long Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
ASTM D-792
Filler Content 50 %
50 %
Long Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength 266 MPa
38600 psi
ASTM D-638
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
ASTM D-638
Tensile Modulus 17.24 GPa
2500 ksi
ASTM D-638
Flexural Strength 369 MPa
53500 psi
ASTM D-790
Flexural Modulus 16.55 GPa
2400 ksi
ASTM D-790
Izod Impact, Notched 3.68 J/cm
6.89 ft-lb/in
ASTM D-256
Izod Impact, Unnotched 12.3 J/cm
23.0 ft-lb/in
ASTM D-4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 254 °C
489 °F
ASTM D-648
Users viewing this material also viewed the following: