Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
PolyOne OnForce™ LFT UR-50 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
RTP Company RTP 1387 HM Polyphenylene Sulfide (PPS) Carbon Fiber 40% - High Modulus
(disco Carbon Fiber 40% - High ModulusComments:Carbon FiberHigh ModulusUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information prov.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
LG Chemical LUMID GP2259AFL PA6+GF25%, Flame Retardant Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Connector)CAS No. 25038-54-4, 65997-17-3, 1163-19-5, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Haysite H515 Polyester, High Temp Flex H515 exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high t.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp KZL34 POM LNP* Lubricomp* KZL34 is a compound based on Acetal resin containing Milled Glass and PTFE. Characteristic of this grade is Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Europe-Africa-Middle East) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | |
Shinil Chemical SHINFLAME PA-66 GF Flame Retardant Polymer Under Hood SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Teknor Apex Chemlon® 233 GVH Nylon 6, 33% Glass Fiber Reinforced Features: Flame Retardant; Good Stiffness; High Strength Processing Method: Injection Method Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ RCP 505C Flame Retardant Concentrate Based In Low-Density Polyethylene Information provided by A. Schulman. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ RCP 500 C DescriptionPolyflam® RCP 500C is an economical flame-retardant concentrate based in low-density polyethylene that features excellent dispersion and processing stability up to 550°F. ApplicationRC.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ RCP 505C Flame Retardant Concentrate Based In Low-Density Polyethylene Information provided by A. Schulman. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Ivory 9035 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 9035 is an ivory color concentrate containing based in polyethylene. This concentrate was designed to provide color and opacity in film and molding applications. POLYBATCH®.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ RCP 500 C DescriptionPolyflam® RCP 500C is an economical flame-retardant concentrate based in low-density polyethylene that features excellent dispersion and processing stability up to 550°F. ApplicationRC.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D 792 |
RTP Company RTP 1103 M 15 BLK Polyethylene Terephthalate (PET), 20% Glass Fiber - 15% Mineral |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | Mixed |
Tra-Con Tra-Bond FS449 Thermally Conductive Epoxy Adhesive TRA-BOND FS449 is a medium viscosity thermally conductive epoxy adhesive that is specifically developed to produce strong, durable high-impact bonds at room temperature which improve heat transfer w.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | |
Tra-Con Tra-Sheet BS Thermally Conductive Sheet TRA-SHEET BS is a thermally conductive and insulated silicone sheet with glass fiber reinforcement. It is suitable for heat dissipation applications for high power devices. Typical applications incl.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | Mixed |
Tra-Con Tra-Cast 3143 Fire Retardant Epoxy Casting Compound TRA-CAST 3143 has a low viscosity and long pot life. It is certified to the requirements of UL 94 V-O, and is recommended for rigid potting, laminating, transformer encapsulating, filament winding a.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Ivory 9035 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 9035 is an ivory color concentrate containing based in polyethylene. This concentrate was designed to provide color and opacity in film and molding applications. POLYBATCH®.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
BLUESTAR 201-G30202 PBT, 30% Glass Filled Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | |
Trelleborg Commercial Neoprene® C644 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Specific Gravity | 1.60 - 1.80 g/cc | 1.60 - 1.80 g/cc | IEC 1212-2 8.1 |
Hippe PF GC 201 Woven Glass Cloth Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. High mechanical strength and good electrical properties under normal humidity. Heat resistant. Information provided by Hippe. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Gromax CCP PBT 3040-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® TK-2046H PCT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D 792 |
RTP Company RTP 801 TFE 20 Acetal (POM), Glass Fiber - PTFE Lubricated |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | |
TSE Industries Son of GLOB™ Millable Urethane Mill Roll Cleaner SON of GLOB is rubber material, based upon our Millathane® millable urethane, which was developed for cleaning mill rolls. SON of GLOB contains an abrasive material which gives it added gusto for c.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
PolyOne Edgetek® PS-20GF/000 FR Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Celanese Celcon® MC270-HM POM, Mineral Reinforced Celcon« MC270-HM is a high modulus, mineral coupled acetal copolymer. It utilizes a higher additive level to provide significant improvement in product stiffness and mold shrinkage and better warp.. |