Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
PolyOne OnForce™ LFT UR-50 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Ovation Polymers Nemcon™ H PC DP120/X2 Polycarbonate, Thermally Conductive Designed for use in high performance electronic assemblies where heat removal is critical to system performance. Combines good thermal conductivity with improved HDT and processability relative to c.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Parker Chomerics THERMATTACH® T422 Thermally Conductive BGA Assembly Tape THERMATTACH have been designed to provide a high performance bond in the assembly of EBGA and TBGA semiconductor packages. Their thermally conductive filler ensures superior package performance whe.. |
|||
Specific Gravity | 1.60 - 1.70 g/cc | 1.60 - 1.70 g/cc | ISO 1183 |
Raschig Group MELOPLAS® 183 MF Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
RTP Company RTP 1303 TFE 15 LE Polyphenylene Sulfide (PPS) Glass Fiber 20% - PTFE 15% - Low Extractable Glass Fiber 20% - PTFE 15% - Low ExtractableComments:Glass FiberPTFE LubricatedLow ExtractableUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affe.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
PolyOne Nymax™ GF 1200 A 55 HS Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D 792 |
RTP Company RTP 4002 FR A HS Polyphthalamide (PPA), Glass Fiber - Flame Retardant - Heat Stabilized |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
DuPont Performance Polymers Rynite® RE5231 BK533 PET
(Unverified Data**) Rynite® RE5231 BK533 is a 35% glass fiber/mica reinforced product modified for improved electrical properties such as dielectric strength.Information provided by DuPont Performance Polymers |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
RTP Company RTP 203G FR HS Nylon 4/6 (PA 4/6) Glass Fiber 20% - Flame Retardant - Heat Stable
&n Glass Fiber 20% - Flame Retardant - Heat StableComments:Glass FiberFlame RetardantHeat Stabilized(Dry As Molded)Unless otherwise specified, all data listed is for natural or black colored materials... |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D297 |
Greene Tweed FLUORAZ® 790 Fluoroelastomer, FEPM Greene, Tweed`s Fluoraz® functions effortlessly in a variety of challenging process environments. Fluoraz performs well in aggressive chemicals where ultrapure materials are not required. Known f.. |
|||
Specific Gravity | 1.60 - 1.70 g/cc | 1.60 - 1.70 g/cc | ASTM D1475 |
Lotus Nano Paint NAX 01 Tow-Component Nano-paint Description: More durable and specific application methods. This paint is suitable for traffic signs on the road, cross-walks, warning vibrating lines and limited lot marking. Related machines could.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-7869/BL PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ISO 1183 |
Gromax CFG45-PN11N1 Nylon 6 46% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ISO 1183 |
Gromax CFG45-PN11N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D 792 |
SABIC Innovative Plastics Valox® 553M PBT+PC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® TK-2046H PCT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D 792 |
RTP Company EMI 331 G FR Polycarbonate (PC), 10% Glass Fiber - Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ RCP 505C Flame Retardant Concentrate Based In Low-Density Polyethylene Information provided by A. Schulman. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ RCP 770C/CW DescriptionPolyflam® RCP 770C/CW is a flame-retardant concentrate based in low-density polyethylene that features excellent dispersion and processing stability up to 550°F.ApplicationRCP 770 C/CW.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | Mixed |
Tra-Con Tra-Bond 2126 Black Opaque Epoxy Adhesive TRA-BOND 2126 is recommended for those modern photographic, industrial, and laboratory bonding and laminating applications where an easy-to-use, black (opaque) epoxy adhesive system with high perfor.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D 792 |
RTP Company RTP 1399 X 130021 A Polyphenylene Sulfide (PPS); Carbon Fiber - Glass Fiber - Electrically Conductive - (Preliminary Data) |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Cheng Yu Plastic NG1500S Nylon 66, 50% Glass Fiber Reinforced |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Cheng Yu Plastic T885GV3 Flame Retardant PBT, 30% Glass Fiber |
|||
Specific Gravity | 1.60 - 1.90 g/cc | 1.60 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe SI GC 201 Woven Glass Cloth Reinforced Silicone Resin - Sheet Used in electrical and electronic applications. Extremely good electrical properties under dry conditions; good properties under humid conditions.Information provided by Hippe. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D-792 |
PlastiComp Complet® LGF50 - PA66 Nylon 66, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Celanese Celcon® MC270-HM POM, Mineral Reinforced
(Unverified Data**) Celcon® MC270-HM is a high modulus, mineral coupled acetal copolymer. It utilizes a higher additive level to provide significant improvement in product stiffness and mold shrinkage and better warp.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Celanese Impet® 830R PET, 35% Mineral / Glass Reinforced
(Unverified Data**) Impet 830R is a 35% glass/mineral reinforced injection moldable polyester made with recycled PET. It provides an excellent combination of strength, stiffness, warp resistance, and high temperature c.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Celanese FORTRON 1130L4 PPS, 30% Glass Reinforced
(Unverified Data**) Fortron 1130L4 is a 30% glass-reinforced PPS that has excellent heat and chemical resistance. It is inherently flame-retardant and exhibits high hardness and a good balance of strength and stiffness.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Celanese Celcon® MC90-HM POM, Mineral Reinforced Celcon« MC90-HM is a highly mineral filled and coupled M90 material for producing very flat and dimensionally stable parts (normal flow).Information provided by Celanese |