PlastxWorld CEVIAN® B1500 PBT/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN® B1500 PBT/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unfilled, Excellent ToughnessThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
ASTM D955
Melt Flow 15 g/10 min
15 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength, Yield 42.1 MPa
6100 psi
ASTM 638
Elongation at Break 100 %
100 %
ASTM D638
Flexural Yield Strength 62.7 MPa
9100 psi
ASTM D790
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.17 mm
1.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
0.25 inch; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
0.25 inch; ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: