Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 62.7 MPa | 9100 psi | ASTM D790 |
Ravago Manufacturing Americas Hylac® LG35 Low Gloss ABS Acrylonitrile Butadiene Styrene, low gloss ABS.Information provided by Ravago. |
|||
Flexural Yield Strength | 62.8 MPa | 9100 psi | ASTM D790 |
Iran Petrochemical (PCC) SD-0150 Acrylonitrile Butadiene Styrene General Purpose ABS, SD 0150 grade, is a rigid thermoplastic with good processing characteristics. It is a high flow injection molding grade with considerable impact strength and medium heat deflec.. |
|||
Flexural Yield Strength | 62.7 MPa | 9100 psi | ASTM D790 |
Spartech Millennium IV Glass Filled ABS Structural Sheet Description: Structural SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 62.7 MPa | 9100 psi | ASTM D790 |
Techmer ES Luriblend® TPU T/AL27 Aramid Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid Fiber FilledAdditive: PTFE LubricantFeatures: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 62.7 MPa | 9100 psi | ASTM D790 |
PlastxWorld CEVIAN® B1500 PBT/ABS Alloy Unfilled, Excellent ToughnessThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 62.8 MPa @Thickness 6.40 mm |
9100 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU602 ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Flexural Yield Strength | 62.8 MPa @Thickness 6.40 mm |
9100 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron SE-22 ABS Sheet Extrusion Grade Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali |
|||
Flexural Yield Strength | 62.8 MPa @Thickness 6.40 mm |
9100 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron SE-22 ABS Sheet Extrusion Grade Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali |
|||
Flexural Yield Strength | 62.8 MPa @Thickness 6.40 mm |
9100 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron SHF-50+ ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Flexural Yield Strength | 62.8 MPa @Thickness 6.40 mm |
9100 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron SHF-50+ ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Flexural Yield Strength | 62.8 MPa @Thickness 6.40 mm |
9100 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU602 ABS Heat Resistant High ImpactInformation provided by Bhansali |