Material Notes:
Glass fiber reinforced and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
24 hr; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Yield 73.8 MPa
10700 psi
ASTM 638
Flexural Yield Strength 97.9 MPa
14200 psi
ASTM D790
Flexural Modulus 5.88 GPa
853 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm

@Thickness 3.17 mm
1.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.6 µm/m-°C

@Temperature 20.0 °C
17.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C
207 °F
0.5 inch unannealed; ASTM D648
Vicat Softening Point 103 °C
217 °F
ASTM D1525
Flammability, UL94 V-0

@Thickness 1.70 mm
V-0

@Thickness 0.0669 in