PlastxWorld Veroplas PA2009L Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer PlastxWorld, Inc.
Trade Name Veroplas
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld Veroplas PA2009L Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
general purpose, super lubricated injection molding gradeInformation provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM A792
Moisture Absorption at Equilibrium <= 0.17 %
<= 0.17 %
Karl Fischer
Linear Mold Shrinkage 0.024 cm/cm
0.024 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 68.3 MPa
9900 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Yield Strength 77.9 MPa
11300 psi
ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
ASTM D790
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C
120 °F
ASTM D648
Vicat Softening Point 171 °C
340 °F
ASTM D1525
Glow Wire Test 649 °C
1200 °F
UNE 20-672-83