Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastxWorld Veroplas PA3301F Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Fiber Filled, Flame Retardant
Manufacturer PlastxWorld, Inc.
Trade Name Veroplas
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld Veroplas PA3301F Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
flame retarded (UL94 V0), 30% glass filled injection molding gradeInformation provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ASTM A792
Moisture Absorption at Equilibrium <= 0.17 %
<= 0.17 %
Karl Fischer
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 110 MPa
16000 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Yield Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 5.50 GPa
798 ksi
ASTM D790
Izod Impact, Notched 0.998 J/cm
1.87 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ASTM D648
Vicat Softening Point 232 °C
450 °F
ASTM D1525
Flammability, UL94 V-0

@Thickness 2.50 mm
V-0

@Thickness 0.0984 in
Glow Wire Test 960 °C
1760 °F
UNE 20-672-83
Users viewing this material also viewed the following: