Material Notes:
general purpose, 40% glass filled injection molding gradeInformation provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM A792
Moisture Absorption at Equilibrium <= 0.17 %
<= 0.17 %
Karl Fischer
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 190 MPa
27600 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Yield Strength 240 MPa
34800 psi
ASTM D790
Flexural Modulus 8.00 GPa
1160 ksi
ASTM D790
Izod Impact, Notched 1.77 J/cm
3.31 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 229 °C
444 °F
ASTM D648
Vicat Softening Point 249 °C
480 °F
ASTM D1525
Glow Wire Test 649 °C
1200 °F
UNE 20-672-83