Plenco 3356 Phenolic, Granular, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 3356 Phenolic, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.660 g/cc
0.0238 lb/in³
ASTM D1895
Density 1.57 g/cc
0.0567 lb/in³
ASTM D792
Water Absorption 0.181 %
0.181 %
ASTM D570
Linear Mold Shrinkage 0.0043 cm/cm
0.0043 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 78
78
ASTM D785
Tensile Strength, Ultimate 46.0 MPa
6670 psi
ASTM D638
Elongation at Break 0.52 %
0.52 %
ASTM D638
Tensile Modulus 10.2 GPa
1480 ksi
ASTM D638
Flexural Strength 86.0 MPa
12500 psi
ASTM D790
Flexural Modulus 10.3 GPa
1490 ksi
ASTM D790
Compressive Strength 159 MPa
23100 psi
ASTM D695
Izod Impact, Notched 0.205 J/cm
0.384 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.212 J/cm²
1.01 ft-lb/in²
ASTM D256
Impact 89
89
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 56.0 µm/m-°C

@Temperature 40.0 - 130 °C
31.1 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 208 °C
406 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Shrinkage 0.147 %
0.147 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 4.50e+11 ohm-cm
4.50e+11 ohm-cm
ASTM D247
Dielectric Constant 5.4
5.4
ASTM D150
Dielectric Strength 7.70 kV/mm
196 kV/in
Step by Step; ASTM D149
11.5 kV/mm
292 kV/in
Short Time; ASTM D149
Dissipation Factor 0.062
0.062
ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638