Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ASTM D638-95 |
Multibase Multi-Pro® 2005 XRC Black 20% Filler Content Polypropylene Multi-Pro 2005 XRC is specifically designed for injection molded electronic industrial uses. This product shows higher heat distortion and notched izod than typical glass filled polypropylene. Thi.. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ISO 527 |
LATI LATILUB 73/13-10ST Polyoxymethylene Base (POM), 10% Mixed PTFE/Silicone Self Lubricating Plastic
(Un Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ASTM D638 |
Plenco 6802 Phenolic, Granular, Transfer Molded
(discontinued **) Two-Stage Phenolic. PLENCO 06802 is a mica and mineral filled novolac phenolic molding compound. Available in Brown.Information supplied by Plenco |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ASTM D638 |
Plenco 5314 Black (COM) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 5314 is the replacement material for the former Union Carbide BMMA-5314. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Tensile Strength, Ultimate | 46.0 MPa @Temperature 1150 °C |
6670 psi @Temperature 2100 °F |
|
Haynes 214® alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Tensile Strength, Ultimate | 46.0 MPa @Temperature 1149 °C |
6670 psi @Temperature 2100 °F |
|
Haynes HR-160® alloy, solution annealed sheet Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ASTM D638 |
Plenco 3356 Phenolic, Granular, Transfer Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ASTM D638 |
Plenco 4349 Phenolic, Granular, Compression Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ASTM D638 |
Plenco 4466 Phenolic, Granular, Compression Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | 5mm/min; ISO 527-1, 2 |
Polyplastics TOPAS® 5013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) This grade is characterized by its high flowability and superior optical properties. It is suitable for optical components such as lenses and light guide panels where high molded precision is indisp.. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ISO 37 |
Lubrizol ESTANE® GP55DT Ether Based Thermoplastic Polyurethane Type: Estane® GP 55DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in .. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | DIN 53504 |
Lubrizol ESTANE® 58447 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ISO 527 |
Eastman DURASTAR DS1010 Natural PCTA Copolyester DURASTAR DS1010 polymer contains a mold release. It has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to .. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ISO 527 |
Eastman Eastar Copolyester BR003, Natural PCTA Copolyester EASTAR BR003 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabiliti.. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ISO R527 |
Arkema Group Orgalloy® LE 60LMXV Polyamide 6 Alloy Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | |
BASF Polystyrol® 143 E Polystyrene (Europe) Medium strength, easy flowing general-purpose grade, suitable for blending with impact-modified Polystyrol, Styrolux and as a coextruded glossy capping layer.Data was collected by ISO methods and pr.. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 131 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | |
BASF Polystyrol® 143 EO Polystyrene (Europe) Easy flowing grade for the injection molding and extrusion of low-taint food packaging.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ATSM D638 |
Ashley Polymers Ashlene® 256 PPO A general purpose grade with good heat resistance and impact strength. Other properties include dimensional stability and moisture resistance.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ATSM D638 |
Ashley Polymers Ashlene® PPO 263 A general purpose grade with good heat resistance and impact strength. Other properties include dimensional stability and moisture resistance.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ATSM D638 |
Ashley Polymers Ashlene® T940H Nylon 11 A general purpose, highly flexible Natural Nylon 11 resin with UV stabilizers.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 121 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.11% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ASTM D638 |
Toyobo A1061D Thermoplastic Polyurethane Elastomer, Injection Grade Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes,.. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | XY direction; ASTM D638 |
ALM D80-ST Nylon 11 SLS Prototyping Polymer Unfilled, color stabilized nylon 11 material that is also stabilized to prevent premature thermal degradation. Parts produced from PA D80-ST exhibit superior mechanical properties. Relatively inexp.. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ASTM D412 |
BASF Elastollan® 685A10 Polyester Type Polyurethane Elastomer This grade contains a hydrolytic stabilizer. The Elastollan 600 Series of products listed are products that are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are .. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | DIN 53504 |
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 46.0 MPa @Temperature 60.0 °C |
6670 psi @Temperature 140 °F |
ISO 527 |
LATI LARIL 13 Light Brown Polyphenylene Oxide (PPOm)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Tensile Strength, Ultimate | 46.0 MPa | 6670 psi | ASTM D638 |
Plaslok 5314 Black (COM) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5314 is the replacement material for .. |