Plenco 4300 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Cellulose Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 4300 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electrical control applications. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04300 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.720 g/cc
0.0260 lb/in³
ASTM D1895
Density 1.57 g/cc
0.0567 lb/in³
ASTM D792
Water Absorption 0.18 %
0.18 %
ASTM D570
Linear Mold Shrinkage 0.0031 cm/cm
0.0031 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 84
84
ASTM D785
Tensile Strength, Ultimate 44.0 MPa
6380 psi
ASTM D638
Elongation at Break 0.44 %
0.44 %
ASTM D638
Tensile Modulus 11.0 GPa
1600 ksi
ASTM D638
Flexural Strength 76.0 MPa
11000 psi
ASTM D790
Flexural Modulus 10.5 GPa
1520 ksi
ASTM D790
Compressive Strength 195 MPa
28300 psi
ASTM D695
Izod Impact, Notched 0.160 J/cm
0.300 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.208 J/cm²
0.990 ft-lb/in²
ASTM D256
Impact 102
102
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 52.0 µm/m-°C

@Temperature 40.0 - 130 °C
28.9 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.540 W/m-K

@Temperature 100 °C
3.75 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 203 °C
397 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 197 °C
387 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Oxygen Index 28 %
28 %
ASTM D2863
Shrinkage 0.112 %
0.112 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.50e+12 ohm-cm
2.50e+12 ohm-cm
ASTM D247
Dielectric Constant 5.1
5.1
ASTM D150
Dielectric Strength 14.9 kV/mm
378 kV/in
Short Time; ASTM D149
Dissipation Factor 0.038
0.038
ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638