Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.5 GPa @Temperature 23.0 °C |
1520 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANAMID 66 A12^ F35 NH9 Nylon 66, Glass Fiber Reinforced, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Flexural Modulus | 10.5 GPa @Temperature 23.0 °C |
1520 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ASTM D790 |
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ISO 178 |
Grupo Repol Dinalon® A1S25 G50 PA66 50% Glass Fiber Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ISO 178 |
Solvay TECHNYL® C 216 V35 Black Z PA6, 35% glass fiber, DRY Description: Polyamide PA6 , reinforced with 35 % of glass fiber, for injection molding.Available in: North AmericaProduct Applications: It has good mechanical properties, it is used in all sectors .. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ASTM D790 |
Plenco 1500 Polyester, Granular, Transfer Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ASTM D790 |
Plenco 3303 Phenolic, Granular, Compression Molded Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | dry; ISO 178 |
DSM EcoPaXX® Q-X07209 PA410-I-GF40 % Glass Reinforced, Impact Modified |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | dry; ISO 178 |
DSM Stanyl® TW241B3 PA46-CF15 15% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ISO 178 |
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® HTN 51G35HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL NC010 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ISO 178 |
Eurotec® Tecomid® NB40 GR50 NL PA 6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R535H NT651 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535H NT651 is 35% glass-fiber reinforced PA66 resin. Available in natural, it is heat-stabilized with an electrically neutral heat stabilizer. It is designed specially for electrical appli.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ASTM D790 |
Beijing Ranger Chem PBT 403 G-M50 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ASTM D790 |
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material Product Introduction: Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC t.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 640 Nylon 6/12, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ISO 178 |
DuPont Performance Polymers Rynite® FR530L BK507 Polyethylene Terephthalate (PET) Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 10.5 GPa @Temperature 60.0 °C |
1520 ksi @Temperature 140 °F |
ASTM D790 |
LATI LARTON G/30 30% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Flexural Modulus | 10.5 GPa @Temperature 90.0 °C |
1520 ksi @Temperature 194 °F |
ASTM D790 |
LATI LARTON G/40 40% Glass Fiber Filled Polyphenylene sulfide (PPS)
(Unverified Data**) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |