Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 4504 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Cellulose Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 4504 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding compounds. Since it also has good electrical properties, it has found use in a wide variety of wiring device applications. It is UL recognized under file E40654.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.660 g/cc
0.0238 lb/in³
ASTM D1895
Density 1.57 g/cc
0.0567 lb/in³
ASTM D792
Water Absorption 0.223 %
0.223 %
ASTM D570
Linear Mold Shrinkage 0.00283 cm/cm
0.00283 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 83
83
ASTM D785
Tensile Strength, Ultimate 49.0 MPa
7110 psi
ASTM D638
Elongation at Break 0.51 %
0.51 %
ASTM D638
Tensile Modulus 11.3 GPa
1640 ksi
ASTM D638
Flexural Strength 74.0 MPa
10700 psi
ASTM D790
Flexural Modulus 9.80 GPa
1420 ksi
ASTM D790
Compressive Strength 183 MPa
26500 psi
ASTM D695
Izod Impact, Notched 0.174 J/cm
0.326 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.207 J/cm²
0.985 ft-lb/in²
ASTM D256
Impact 98
98
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 191 °C
376 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Shrinkage 0.127 %
0.127 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+12 ohm-cm
3.00e+12 ohm-cm
ASTM D247
Dielectric Constant 5.1
5.1
ASTM D150
Dielectric Strength 13.1 kV/mm
333 kV/in
Short Time; ASTM D149
Dissipation Factor 0.044
0.044
ASTM D150
Arc Resistance 171 sec
171 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638
Users viewing this material also viewed the following: