Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Greenflex® HN 70 Ethylene Vinyl Acetate Copolymer - Compounding

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Greenflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Greenflex® HN 70 Ethylene Vinyl Acetate Copolymer - Compounding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Greenflex HN 70 is an ethylene vinyl acetate copolymer (EVA) for compounding applications. Greenflex HN 70 is a medium fluidity grade with high tack.Main Applications: Greenflex HN 70 is recommended as base component for hot melt adhesives used in packaging, bookbinding and woodworking.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.952 g/cc
0.952 g/cc
ISO 1183
Vinyl Acetate Content 28 %
28 %
Internal Method
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ISO 868/A
Hardness, Shore D 31
31
ISO 868/A
Tensile Strength, Yield 2.70 MPa
392 psi
ISO 527
Flexural Modulus 0.0150 GPa
2.18 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 73.0 °C
163 °F
Internal Method
Vicat Softening Point 45.0 °C

@Load 1.00 kg
113 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746