Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Greenflex® ML 30 Ethylene Vinyl Acetate Copolymer - Injection Molding & Profile Extrusion

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Greenflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Greenflex® ML 30 Ethylene Vinyl Acetate Copolymer - Injection Molding & Profile Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Greenflex ML 30 is an ethylene vinyl acetate copolymer (EVA) for injection molding and profile extrusion. Items produced with Greenflex ML 30 show good ESCR and elasticity.Main Applications: Greenflex ML 30 is recommended for the production of gaskets, especially if food contact is required, profiles and flexible items.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.929 g/cc
0.929 g/cc
ISO 1183
Vinyl Acetate Content 9.0 %
9.0 %
Internal Method
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
ISO 868/A
Hardness, Shore D 42
42
ISO 868/A
Tensile Strength, Yield 6.50 MPa
943 psi
ISO 527
Flexural Modulus 0.0900 GPa
13.1 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 97.0 °C
207 °F
Internal Method
Vicat Softening Point 72.0 °C

@Load 1.00 kg
162 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746