Polymer Property : Specific Gravity = 0.929 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.929 g/cc
0.929 g/cc
23/23°C; ASTM D792
RheTech Products E206-01 Linear Low Density Polyethylene, Black
Applications: Flexible componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Specific Gravity 0.929 g/cc
0.929 g/cc
ISO 1183
Polimeri Europa Greenflex® FF 35 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FF 35 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. The resin shows good strechability and sealability.Main Applications: Greenflex FF 35 is suitable for flexibl..
Specific Gravity 0.929 g/cc
0.929 g/cc
ISO 1183
Polimeri Europa Greenflex® ML 30 Ethylene Vinyl Acetate Copolymer - Injection Molding & Profile Extrusion
Greenflex ML 30 is an ethylene vinyl acetate copolymer (EVA) for injection molding and profile extrusion. Items produced with Greenflex ML 30 show good ESCR and elasticity.Main Applications: Green..
Specific Gravity 0.929 g/cc
0.929 g/cc
ISO 1183
Polimeri Europa Greenflex® ML 31 Ethylene Vinyl Acetate Copolymer - Injection Molding & Profile Extrusion
Greenflex ML 31 is an ethylene vinyl acetate copolymer (EVA) for injection molding applications and extrusion profile. Greenflex ML 31 contains additive waxes to obtain high production speed.Main A..
Specific Gravity 0.929 g/cc
0.929 g/cc
ISO 1183
Polimeri Europa Greenflex® MP 34 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding
Greenflex MP 34 is an ethylene vinyl acetate copolymer (EVA) for injection molding and compounding applications. Greenflex MP 34 combines high fluidity with high elasticity.Main Applications: Gree..
Specific Gravity 0.929 g/cc
0.929 g/cc
Teknor Apex TruVis Esters™ DIOA Di-IsoOctyl Adipate
Specific Gravity 0.929 g/cc
0.929 g/cc
ISO 1183
Total EVA 1010 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1010 VN 3 is made by a high pressure tubular process. Grade for films with high transparency and high mechanical properties. Contains an antioxidant.Application examples: Stretch film, food pa..
Specific Gravity 0.929 g/cc
0.929 g/cc
ISO 1183
Total EVA 1020 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1020 VN 3 is made by a high pressure tubular process. Grade for flexible, very transparent films with high strength and very good sealability. Contains an antioxidant.Application examples: Thi..