Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyMirae Moplen HP652P Fiber (BCF/CF) Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen HP652P Fiber (BCF/CF) Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen HP652P is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP652P is a homopolymer particularly suitable for heavy denier BCF and CF multi-filament. Moplen HP652P resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520.Features: Excellent spinnability; Excellent drawability; Outstanding gloss and surface appearanceApplications: BCF/Multi-Filament; Automobile Interior stuffs; IndustrialInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 37.3 MPa
5400 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.67 GPa
242 ksi
ASTM D790
Izod Impact, Notched 0.294 J/cm
0.551 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C
223 °F
ASTM D648
Vicat Softening Point 155 °C
311 °F
ASTM D1525
Users viewing this material also viewed the following: