Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.67 GPa | 242 ksi | STN EN ISO 178 |
Plastcom PLASTAMID® 610 BT N 32 C PA610 Basic type PA610 for injection molding, modified for general use. Use: extrusion, filaments, injection molding. Delivered in the natural color.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | ASTM D790 |
PolyMirae Moplen EP640T Injection Molding Grade Polypropylene Moplen EP640T is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP640T is a block copolymer suitable for injection molding of a.. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | ASTM D790 |
PolyMirae Moplen HP600R Injection Grade Polypropylene Moplen HP600R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP600R is a homopolymer typically used in injection molding of food.. |
|||
Flexural Modulus | 1.67 - 2.00 GPa | 242 - 290 ksi | Average value: 1.87 GPa Grade Count:13 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | ASTM D790 |
Hyosung Topilene HJ640 PP HJ640 High Isostatic PP Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporatio.. |
|||
Flexural Modulus | 1.67 GPa @Thickness 3.20 mm |
242 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical ALPHALAC SH860 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Refrigerator Inner LinerCAS No. 9003-55-8Information provided by LG Chemical |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | ASTM D790 |
Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Flexural Modulus | 1.67 GPa @Thickness 3.20 mm |
242 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP5008A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, High FlowApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® 6431 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® 6531M Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® PD943 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | ASTM D790 |
KKPC Kuhmo HI 425EH Extrusion Molding HIPS Key features: ESCR Common Uses: Refrigerator inner liners, door liners, disposable cups, food packaging sheet, wrapping films, trays, washing machinesHIPS is a functional resin made by copolymerizat.. |
|||
Flexural Modulus | 1.67 GPa @Thickness 6.40 mm |
242 ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL MC4352 PP+Rubber+MF Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, Scratch resistance, Good Weatherability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9.. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp ML002S PP LNP* Lubricomp* ML002S is a compound based on Polypropylene containing PTFE. Characteristics of this grade are: Heat Stabilized and Internally Lubricated.This data was supplied by SABIC-IP for the.. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | |
Shinil Chemical SHINNANO PP Polymer Nanocomposite Door Trim SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | |
Shinil Chemical SHINSTAT PCTG Electrostatic Control Polymer Sheet Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | |
Shinil Chemical SHINSTAT PE Electrostatic Control Polymer Sheet Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SD-0170 ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9750H ASA, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SD-0170 ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SD-0190H ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HN-1064IA PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.67 GPa @Thickness 3.20 mm |
242 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SPEXP 44 Antistatic Polystyrene Characteristics Easy flow Good transparency Very good flexibility Processing Extrusion Applications Transparent profiles for electrostatic dissipative packaging of small electronic components such.. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P600F Polypropylene Film Resin Key Characteristics:Good optical propertiesHigh productivityGood openability with 3000 ppm slip agent and 2700 ppm antiblocking agentRecommended Applications:Water quenched blown film for food and a.. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P602F Polypropylene Film Resin Key Characteristics:Excellent optical propertiesHigh productivityRecommended Applications:Water quenched blown film for food and apparel packagingCan be blended with P600 for excellent clarityInform.. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P702J Polypropylene Injection Molding Key Characteristics:High clarityHigh stiffnessGood processabilityMicrowavable for cooking applicationsOdorlessSafe for food contactRecommended Applications:General purpose injection parts that requi.. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | |
Zylog Hipolyene® X2 DP 4 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | 50 mm/min; ASTM D790 |
3M Dyneon™ PVDF 2066_0002 Fluoroplastic 3M™ Dyneon™ PVDF 2066/0002, a fluoropolymer material, provides an excellent balance of physical properties, processability, surface smoothness, flexibility, and refractive index, allowing for a wi.. |
|||
Flexural Modulus | 1.67 GPa | 242 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HN-1064IA PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.67 - 82.7 GPa | 243 - 12000 ksi | Average value: 8.92 GPa Grade Count:42 |