Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® AS-40GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® AS-40GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.371 g/cc
1.371 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0015 - 0.0020 cm/cm
0.0015 - 0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 75.8 MPa
11000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 7.79 GPa
1130 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 7.79 GPa
1130 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.50 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Processing Properties Metric English Comments
Melt Temperature 221 - 249 °C
430 - 480 °F
Molding
Mold Temperature >= 65.6 °C
>= 150 °F
Drying Temperature 65.6 °C
150 °F
Dry Time 6 hour
6 hour
Descriptive Properties Value Comments
Product Form Pellets