Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® PK-30GF/000 HT Polyaryletherketone, Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Polyketone
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® PK-30GF/000 HT Polyaryletherketone, Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:30% Glass FilledPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.54 g/cc
1.54 g/cc
ASTM D792
Water Absorption 0.10 %

@Thickness 3.17 mm
0.10 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 165 MPa
24000 psi
Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 11.7 GPa
1700 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 248 MPa
36000 psi
ASTM D790
Flexural Modulus 10.3 GPa
1500 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
2.10 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 310 °C
590 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 388 - 399 °C
730 - 750 °F
Molding
Users viewing this material also viewed the following: