Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ 170 Series 173 Polyvinyl Chloride Homopolymer (PVC Homopolymer)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ 170 Series 173 Polyvinyl Chloride Homopolymer (PVC Homopolymer).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron® 940. Note: The values set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Density 0.320 - 0.400 g/cc
0.0116 - 0.0145 lb/in³
ASTM D1505
Fineness 5.5
5.5
North Fineness; Geon® 390
Relative Viscosity 2.37 cP
2.37 cP
1% Cyclohexanone
Brookfield Viscosity 2.55 cP
2.55 cP
Initial, V12, Geon® 1010
3.6 cP
3.6 cP
One Day, V12, Geon® 1010
Viscosity Measurement 1.0
1.0
Inherent; ASTM D1243-60-A
Melt Flow 270 g/10 min

@Pressure 0.655 MPa
270 g/10 min

@Pressure 95.0 psi
Severs Efflux; Geon® 1010
Mechanical Properties Metric English Comments
Tensile Strength 16.5 MPa
2390 psi
Optimum; FF; ASTM D638
Elongation at Yield 350 %
350 %
FF; Optimum Tensile; ASTM D412
Optical Properties Metric English Comments
Gloss 93 %
93 %
60°, FF, ALTC-65
Transmission, Visible 86 %
86 %
FF, ATLC-66
Processing Properties Metric English Comments
Moisture Content 0.050 %
0.050 %
Karl Fisher-Geon® 683
Descriptive Properties Value Comments
Degree of Polymerization 1250
Correlation
Features Low to No Odor
Low to No Taste
Resilient
Forms Powder
Gel Temperature 79 °C
FF, ALTC-29
Generic Material PVC Homopolymer
Generic Name Polyvinyl Chloride Homopolymer (PVC Homopolymer)
K-Value 69
No Standard; Correlation
Methanol Extractables 1.1%
Geon® 894
Polymerization Process Dispersion
Processing Method Casting
Dip Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Coating Applications
Film
Users viewing this material also viewed the following: