Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.320 g/cc | 0.0116 lb/in³ | ASTM D3574 |
Rogers Corporation Bisco™ HT-800 Cellular Silicone Foam Medium grade silicon sponge. UL recognized for flame retardance and gasketing.Applications: HID (High Intensity Discharge) lighting fixture gaskets, Battery cushion in hand-held electronic products.. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | ±10%; ASTM D3574A |
Rogers Corporation Poron® 4701-30-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4701-30-20 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which ena.. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4701-30-20064 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement. Standard available thickness 0.064"Features and Benefits of PORON Products: Excelle.. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® 4701-41-20 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation Poron® Shock Seal™ 4790-79-20 Urethane Foam, Industrial Grade Thickness: 0.062"- 0.188"Color: BlackInformation provided by Rogers Corporation. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | ASTM D3574-95 Test A |
Rogers Corporation R/bak® SS Cushion Mounting Materials, Supported Soft R/bak materials are high-density, open cell, polyurethane foams used to build thickness on the cylinder, provide cushioning and absorb vibration in the Flexographic printing process. The use of R/b.. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | Free Rise Density |
Northstar Polymers MPL-R20B Rigid Polyurethane Foam Formulation This rigid polyurethane foam system is one of a family of polymer systems developed by Northstar Polymers for specific applications. Urethane foams molded with this system exhibit closed cell struct.. |
|||
Density | 0.320 - 0.400 g/cc | 0.0116 - 0.0145 lb/in³ | ASTM D1505 |
PolyOne Geon™ 170 Series 179 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron®.. |
|||
Density | 0.320 - 0.350 g/cc | 0.0116 - 0.0126 lb/in³ | |
Microtherm Group Molded Pipe Sections Filament Reinforced Silica Pipe Insulation Microtherm® Moulded Pipe Sections (MPS) are preformed pieces of pipe insulation designed to provide a thermally efficient insulation system for piping of all sizes from 25 mm (1â€) upwards. F.. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | |
Sawbones Second-Generation Simulated Cancellous Bone (Cellular) Rigid Polyurethane BoneSawbones® Second-Generation composite bone is a combination of e-glass cloth, mat, and roving, layered around a rigid polyurethane foam core, which models the cancellous ma.. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | |
Sawbones Solid Rigid Polyurethane Foam 20 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | ASTM D792 |
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 20 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Density | 0.320 - 0.380 g/cc | 0.0116 - 0.0137 lb/in³ | ISO 1183 |
Fainplast Compounds EVAtech 803S Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | |
3M 12049 Black 3/8" (9.5 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | foam with adhesive; ASTM D3574 |
3M 4504 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | ASTM D3574 |
3M 4508 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | Typical, 3M QCM 14.24.6 |
3M HGS2000 Glass Bubbles 3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of.. |
|||
Density | 0.320 - 0.380 g/cc | 0.0116 - 0.0137 lb/in³ | |
3M S35 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | Foam |
Aptek DI-STRATE 95211 Microwave/RF Foam Substrate DI-STRATE™ Tiles are fully-crosslinked, low density, composite foam substrates which exhibit a low characteristics in the microwave frequency range.Uses: Space AntennasInformation provided by Aptek.. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | |
3M 12048 Black 1/8" (3.2 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | |
3M 12054 Black 1/4" (6.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | foam with adhesive; ASTM D3574 |
3M 4508 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | |
Zircar Ceramics ASH Alumina-Silica Insulation ZIRCAR Ceramics Alumina-Silica Insulation Type ASH is one of the first alumina-silica products produced by ZIRCAR. Made of bulk fiber and inorganic alumina binders Type ASH is uniform throughout its.. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | ASTM D1622 |
Touchstone CFOAM® 20 Structural Carbon Foam CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins.. |
|||
Density | 0.320 g/cc | 0.0116 lb/in³ | ±10%; ASTM D3574A |
Rogers Corporation Poron® 4701-40-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |