Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 16.5 MPa | 2390 psi | ASTM D2095 |
Permabond UV625 UV-curable Adhesive PERMABOND UV625 is a single part, fast curing, UV curable adhesive primarily designed for bonding and sealing glass and metal. The cured adhesive is tough, flexible and has excellent impact resistan.. |
|||
Tensile Strength | 16.5 MPa | 2390 psi | Optimum; FF; ASTM D638 |
PolyOne Geon™ 170 Series 173 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron®.. |
|||
Tensile Strength | 16.5 MPa | 2400 psi | Typical |
Garlock 7164 SBR Rubber Lining SBR rubber lining for protection applications such as chute lining and skirtboards.An optional duck fabric backing is available.Information provided by Garlock Rubber Technologies |
|||
Tensile Strength | 16.5 MPa | 2400 psi | ASTM F152 |
Garlock 9064 Neoprene Sheet Rubber Gasketing Neoprene (CR)FDA-approved. Exceptional material for food plants, with superior resistance to most all food products; oily and aqueous.Information provided by Garlock Rubber Technologies |
|||
Tensile Strength | 16.5 MPa | 2390 psi | Dry Heat Aging 392°F; 336 hr; ASTM D865 |
Seals Eastern 5794 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Tensile Strength | >= 16.5 MPa | >= 2400 psi | ASTM D412 Method A |
Seals Eastern 7346 Extreme Low Temperature Service Rubber HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern. |
|||
Tensile Strength | 16.5 MPa | 2400 psi | ASTM D638 |
Teknor Apex APEX® 153 Polyvinyl Chloride Compound Notes: Non-Migrating; Sunlight Resistant Jacket Temperature Rating: 105°CInformation Provided by Teknor Apex |
|||
Tensile Strength | 16.5 MPa | 2400 psi | ASTM D638 |
Teknor Apex APEX® 4157 Polyvinyl Chloride Compound Notes: Non-Migrating; Sunlight Resistant, Tray Cable Jacket Temperature Rating: 105°CInformation Provided by Teknor Apex |
|||
Tensile Strength | 16.5 MPa | 2400 psi | |
Teknor Apex Telcar® TL-3050 Thermoplastic Elastomer Temperature Ratings: Wet Location: 75°C, Dry Location: 90°C Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength | 16.5 MPa | 2390 psi | 300; ISO 37 |
BASF Elastollan 1085 A TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 16.5 MPa | 2390 psi | 20; ISO 37 |
BASF Elastollan 1154 D KFFC TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 16.5 MPa | 2400 psi | |
AlphaGary Garaflex™ E 89-086 C3 NF LCF-R Vinyl Thermoplastic Elastomer Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable105°C rated flexible cord jacket compound |
|||
Tensile Strength | 16.5 MPa | 2390 psi | 500 mm/min, measured parallel to flow; ISO 37 |
AlphaGary Evoprene™ LF 6158 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Tensile Strength | 16.5 MPa | 2400 psi | |
AlphaGary GW 3042 LCF Flame Retardant Polyvinyl Chloride 75°C rated jacket compound |
|||
Tensile Strength | 16.5 MPa | 2400 psi | |
AlphaGary PVC GM 8001-E Natural LCF Polyvinyl Chloride Thermoplastic A lead free, flame retarded, V-O rated compound designed for plug molding |