PolyOne Geon™ Vinyl Flexible A8504 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible A8504 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 79
79
15 sec; ASTM D2240
85
85
ASTM D2240
Tensile Strength at Break 16.9 MPa
2450 psi
510 mm/min; ASTM D638
Tensile Strength 10.3 MPa

@Strain 100 %
1490 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 380 %
380 %
510 mm/min; ASTM D638
Tear Strength 73.6 kN/m
420 pli
Die C, 510 mm/min; ASTM D624
Thermal Properties Metric English Comments
Brittleness Temperature -32.8 °C
-27.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 174 - 179 °C
345 - 354 °F
188 - 199 °C
370 - 390 °F
Descriptive Properties Value Comments
Agency Ratings NSF 61
Potable water material Temperature: Domestic Hot(140F/60C)
Appearance Clear/Transparent
Features General Purpose
High Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Profile Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Appliances
General Purpose
Hose
Tubing