Mechanical Properties Metric English Comments
Tensile Strength at Break 16.9 MPa
2450 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Elastamax™ HTE 3070 Polyvinyl Chloride + NBR (PVC+NBR)
Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a..
Tensile Strength at Break 16.9 MPa
2450 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Elastamax™ HTE 3170 Polyvinyl Chloride + NBR (PVC+NBR)
Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a..
Tensile Strength at Break 16.9 MPa
2450 psi
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible A8504 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 16.9 MPa
2450 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R264AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 16.9 MPa
2450 psi
ASTM D638
Sterigenics Raprex® R100D Branched High Density Polyethylene
Applications: ExtrusionRAPREX® R100D is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique branched struct..
Tensile Strength at Break 16.9 MPa
2450 psi
ASTM D638
Teknor Apex APEX® 3801-75 Polyvinyl Chloride, Flexible
Features: Non-DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex..
Tensile Strength at Break 16.9 MPa
2450 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2174 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FC 2174 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..
Tensile Strength at Break 16.9 MPa
2450 psi
ASTM D638
Teknor Apex APEX® 65009 Polyvinyl Chloride, Flexible
Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex