Material Notes:
Improved adhesion.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm
0.015 - 0.019 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
15 sec; ASTM D2240
70
70
ASTM D2240
Tensile Strength at Break 11.7 MPa
1700 psi
510 mm/min; ASTM D638
Tensile Strength 3.65 MPa

@Strain 100 %
529 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 450 %
450 %
510 mm/min; ASTM D638
Compression Set 18 %

@Temperature 23.0 °C,
Time 79200 sec
18 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Processing Properties Metric English Comments
Melt Temperature 179 - 182 °C
354 - 360 °F
188 - 204 °C
370 - 399 °F
Descriptive Properties Value Comments
Features High Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Seals
Weatherstripping
Users viewing this material also viewed the following: