Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible Y126 White 317 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable 1604-xx07FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable JAC31A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable JAL110A Natural Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1604L-xx07FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1802-xx06FRA Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable W84598L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJAC36L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJJC31L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJJC330 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible A75M1 Trans 9000 Polyvinyl Chloride, Flexible (PVC, Flexible) This compound is certified for fuel hose applications(R1 Type B Class 1)under SAE J 1527 requirements.Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible A9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible B83UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible C90B1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible C90UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible P484 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 182 °C | 354 - 360 °F | |
PolyOne Geon™ Vinyl Flexible R111AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible R5155A White 759 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible R8570B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 166 - 182 °C | 331 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable WR3792CL Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Huntsman PE1033 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good opticals, impact strength, good processing properties, and stiffnessApplications: Film extrusion: general purpose packaging and film applications.FDA No.. |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible B8502 Polyvinyl Chloride, Flexible (PVC, Flexible) A flexible PVC Compound with good resistance to migration to specific applications.Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible B9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible R5230C Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Huntsman PE1257 EVA Film Extrusion
(discontinued **) 2.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, good heat seal characteristics.Applications: Film extrusion: general purpose packaging where to.. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Sylvin Technologies 8600-90 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Sylvin Technologies 8925-90 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Sylvin Technologies 8960-90 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Sylvin Technologies 9925-90 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable 0953-xx04D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |