Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible Y126 White 317 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable 1604-xx07FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable 1741-xx06D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable JJC31A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 182 °C | 331 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable JKC30A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1604L-xx07FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJJC34L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Cellular E2000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Cellular E2001 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible B83UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 179 - 182 °C | 354 - 360 °F | |
PolyOne Geon™ Vinyl Flexible D9501 NATURAL Polyvinyl Chloride, Flexible (PVC, Flexible) A highly filled PVC Compound for extrusion applications.Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible MD403KB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible P484 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible R130AE White 41 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
PolyOne Geon™ Vinyl Flexible R1700D Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible R235AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible R5185A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Huntsman PE1033 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good opticals, impact strength, good processing properties, and stiffnessApplications: Film extrusion: general purpose packaging and film applications.FDA No.. |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible B9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible R5257A White 759 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Huntsman PE1257 EVA Film Extrusion
(discontinued **) 2.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, good heat seal characteristics.Applications: Film extrusion: general purpose packaging where to.. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Huntsman PE1605 EVA Film Extrusion
(discontinued **) 6% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
LyondellBasell Petrothene® YR19548 Polyolefin Compound ApplicationsPETROTHENE YR 19548 is a colorable, thermoplastic non-halogenated, flame retardant polyolefin compound formulated for small gauge automotive primary insulation (SAE J1128) and appliance .. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Sylvin Technologies 8925-90 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Sylvin Technologies 916V0 Black PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Sylvin Technologies 9915-90 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Sylvin Technologies 9940-90 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | |
Sylvin Technologies 9980-90 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 171 - 182 °C | 340 - 360 °F | Molding |
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l.. |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable W3301 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |