PolyOne Geon™ Vinyl Flexible R5155A White 759 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible R5155A White 759 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
15 sec; ASTM D2240
Tensile Strength at Break 8.96 MPa
1300 psi
Type IV, 510 mm/min; ASTM D638
Tensile Strength 3.79 MPa

@Strain 100 %
550 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 380 %
380 %
Type IV, 510 mm/min; ASTM D638
Tear Strength 35.0 kN/m
200 pli
Die C, 510 mm/min; ASTM D624
Thermal Properties Metric English Comments
Brittleness Temperature -48.9 °C
-56.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 177 - 182 °C
351 - 360 °F
193 - 199 °C
379 - 390 °F
Descriptive Properties Value Comments
Additive Biocide
Features Good Weather Resistance
High Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Construction Applications
Outdoor Applications
Seals
Weatherstripping
Users viewing this material also viewed the following: