Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Lubri-Tech™ NL-15KV/000 Nylon 6/12, Aramid Fiber  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Lubri-Tech™ NL-15KV/000 Nylon 6/12, Aramid Fiber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Aramid Fiber ReinforcedInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Water Absorption 0.15 %

@Thickness 3.17 mm
0.15 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.2 MPa
8000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 5.0 %
5.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 2.76 GPa
400 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.20 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 177 °C
350 °F
Unannealed, 0.125 in bars; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C
200 °F
Unannealed, 0.125 in bars; ASTM D648