PolyOne Maxxam™ FR WC 0587-21 R2 RoHS Polypropylene, Unspecified (PP, Unspecified)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer PolyOne Corporation
Trade Name Maxxam™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ FR WC 0587-21 R2 RoHS Polypropylene, Unspecified (PP, Unspecified).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Maxxam FR WC 0587-21 R2 RoHS is a flame retardant polyolefin compound characterized by low flame spread and good processability. Designed for thin wall primary wire applications.UL Yellow Card approval for Plenum cable compounds - Component (E203704)Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.9 MPa
2310 psi
510 mm/minTensile and elongation values are largely determined by processing parameters of the end user.; ASTM D412
Elongation at Break 320 %
320 %
510 mm/minTensile and elongation values are largely determined by processing parameters of the end user.; ASTM D412
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
molded specimen; UL 94
Oxygen Index 34 %
34 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 2.7

@Thickness 2.54 mm
2.7

@Thickness 0.100 in
10 kHz, QuadTech™ Digibridge; ASTM D150
Descriptive Properties Value Comments
Features Flame Retardant
Forms Pellets
Generic Material PP, Unspecified
Generic Name Polypropylene, Unspecified (PP, Unspecified)
Processing Method Extrusion
Regional Availability North America
RoHS Compliance RoHS Compliant
Uses Wire & Cable Applications