PolyOne Maxxam™ MAXBATCH YT-818.G001-1000 Polyethylene, High Density (HDPE)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer PolyOne Corporation
Trade Name Maxxam™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ MAXBATCH YT-818.G001-1000 Polyethylene, High Density (HDPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium carbonate, glass and talc to provide a desired balance of properties including stiffness, durability, impact resistance and heat resistance. Custom grades are available with features such as UV stabilizers, heat stabilizers, custom color, high impact, etc.MAXBATCH PRODUCTInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
Descriptive Properties Value Comments
Appearance Natural Color
Features General Purpose
Filler / Reinforcement Talc Filler
Unspecified FillerReinfor., 70% Filler by Weight
Forms Pellets
Generic Material HDPE
Generic Name Polyethylene, High Density (HDPE)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications