PolyOne Maxxam™ MN-818.S001-8000 Polypropylene, Unspecified (PP, Unspecified)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer PolyOne Corporation
Trade Name Maxxam™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ MN-818.S001-8000 Polypropylene, Unspecified (PP, Unspecified).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium carbonate, glass and talc to provide a desired balance of properties including stiffness, durability, impact resistance and heat resistance. Custom grades are available with features such as UV stabilizers, heat stabilizers, custom color, high impact, etc.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D955
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 82.7 MPa
12000 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 7.0 %
7.0 %
Type I, 51 mm/min; ASTM D638
Flexural Strength 114 MPa
16500 psi
ASTM D790
Flexural Modulus 5.86 GPa
850 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 162 °C

@Thickness 3.18 mm
324 °F

@Thickness 0.125 in
Annealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
ALL; UL 94
Processing Properties Metric English Comments
Mold Temperature 16.0 - 50.0 °C
60.8 - 122 °F
Descriptive Properties Value Comments
Additive UV Stabilizer
Appearance Black
Features General Purpose
Filler / Reinforcement Glass Fiber Reinforcement, 40% Filler by Weight
Forms Pellets
Generic Material PP, Unspecified
Generic Name Polypropylene, Unspecified (PP, Unspecified)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Construction Applications
Consumer Applications
General Purpose
Industrial Applications