PolyOne Maxxam™ PPH-30T Nat Polypropylene Homopolymer (PP Homopolymer)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer PolyOne Corporation
Trade Name Maxxam™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ PPH-30T Nat Polypropylene Homopolymer (PP Homopolymer).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium carbonate, glass and talc to provide a desired balance of properties including stiffness, durability, impact resistance and heat resistance. Custom grades are available with features such as UV stabilizers, heat stabilizers, custom color, high impact, etc.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.7 MPa
4600 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 25 %
25 %
Type I, 51 mm/min; ASTM D638
Flexural Strength 53.1 MPa
7700 psi
ASTM D790
Flexural Modulus 3.72 GPa
540 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.599 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 127 °C

@Thickness 3.18 mm
261 °F

@Thickness 0.125 in
Annealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
ALL; UL 94
Descriptive Properties Value Comments
Appearance Natural Color
Features General Purpose
Homopolymer
Filler / Reinforcement Talc Filler
Unspecified FillerReinfor., 30% Filler by Weight
Forms Pellets
Generic Material PP Homopolymer
Generic Name Polypropylene Homopolymer (PP Homopolymer)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications