Material Notes:
The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part performance. These materials have been specifically formulated to offer ease of processing in most standard thermoplastic processing equipment.Molded Test Bars: Dry as MoldedInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183
Water Absorption 1.0 %
1.0 %
24h/23C; ISO 62
0.80 %

@Thickness 3.18 mm
0.80 %

@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ISO 294-4
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 117 MPa
17000 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Strength, Yield 117 MPa
17000 psi
ISO 527-2
121 MPa
17500 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
Type I, 5.1 mm/min; ASTM D638
2.5 %
2.5 %
ISO 527-2
Tensile Modulus 8.27 GPa
1200 ksi
ASTM D638
8.50 GPa
1230 ksi
ISO 527-2
Flexural Strength 179 MPa
26000 psi
ASTM D790
190 MPa
27600 psi
ISO 178
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
8.40 GPa
1220 ksi
ISO 178
Izod Impact, Notched 0.690 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.29 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
Annealed; ISO 75-2/A
Processing Properties Metric English Comments
Mold Temperature 48.9 - 93.3 °C
120 - 200 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Additive Heat Stabilizer
UV Stabilizer
Appearance Black
Automotive Specifications CHRYSLER MS-DB41 CPN3916
Features General Purpose
Heat Stabilized
Filler / Reinforcement GlassMineral, 40% Filler by Weight
Forms Pellets
Generic Material Nylon 6
Generic Name Polyamide 6 (Nylon 6)
Processing Method Injection Molding
Regional Availability North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications