Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB POLYshine PBT D241 PBT, Impact Modified

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Impact Grade
Manufacturer Polykemi AB
Trade Name POLYshine
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYshine PBT D241 PBT, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Linear Mold Shrinkage 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
With Flow; ISO 2577
0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 37.0 MPa
<= 5370 psi
ISO/R527
Flexural Strength <= 61.0 MPa
<= 8850 psi
ISO 178
Flexural Modulus 1.70 GPa

@Temperature 23.0 °C
247 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
ISO 179
3.50 J/cm²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
120°C/h; ISO 75/1
Vicat Softening Point 160 °C

@Load 5.001 kg
320 °F

@Load 11.03 lb
50°C/h; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
IEC 695-2-1