Polykemi AB SCANAMID 66 A12^ X30 Nylon 66, Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Polykemi AB
Trade Name SCANAMID 66
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB SCANAMID 66 A12^ X30 Nylon 66, Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Filler Content 30 %
30 %
±2%; Polykemi
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 75.0 MPa
<= 10900 psi
ISO/R527
Elongation at Break 5.0 %
5.0 %
ISO/R527
Flexural Strength <= 140 MPa
<= 20300 psi
ISO 178
Flexural Modulus 3.80 GPa

@Temperature 23.0 °C
551 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Glow Wire Test 650 °C

@Thickness 2.00 mm
1200 °F

@Thickness 0.0787 in
IEC 695-2-1