Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Industries Densetec HDPE Marine Board

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Polymer Industries
Trade Name Densetec
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polymer Industries Densetec HDPE Marine Board.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Densetec Marine Board is specially formulated to withstand the rigors of harsh outdoor marine environments. It is UV-stabilized to resist damage and retain its beauty, even after years of direct sunlight. Increasingly, Densetec Marine Board is replacing wood and laminates in boating applications. It does not splinter, crack, delaminate, rot, swell, or absorb water like traditional materials.Information provided by Polymer Industries.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D1505
ESCR 100% Igepal® 35 hour
35 hour
CO-630; Condition B; ASTM D1693
45 hour
45 hour
CO-630; Condition A; ASTM D1693
Melt Index of Compound 0.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
2in (50mm) per min.; ASTM D638 Type 4
Elongation at Break >= 600 %
>= 600 %
2in (50mm) per min.; ASTM D638 Type 4
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 126 µm/m-°C

@Temperature 20.0 °C
70.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Brittleness Temperature <= -84.0 °C
<= -119 °F
ASTM D746
Flammability, UL94 HB
HB
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved